Temporal Aspects of the Quality of the Permanent Dentures: a Combination of Structural Materials

Z. R. Ozhohan, A. V. Biben

Abstract


Data on the quality and duration of using permanent dentures made from different structural materials under condition of combination on the teeth antagonists were analyzed. Tribological characteristics of all metal dentures are high, but they do not meet aesthetic and functional requirements and permanent dentures with ceramic coating cause significant abrasion of the antagonist teeth. Several studies indicated that zirconium dioxide dentures do not cause any abrasion of the antagonist teeth, they are aesthetic and bioinert.

 


Keywords


permanent dentures; metal-ceramic construction; zirconium dioxide; dental hard tissues

Full Text:

PDF

References


Pavlenko A.V., Timofeyev A.A. Changes in a patient’s body during prolonged use of permanent dentures. Zbirka naukovykh prats Instytutu stomatolohii KMAPO im. P.L. Shupyka. Kyiv. 2004; 1: 126-128.

Beloklitskaya G.F., Gurenok V.I. Treatment of non-carious lesions of dental hard tissues using “VOCO” materials. Sovremennaya stomatologiya. 2002; 2: 23-26.

Borysenko A.V., Pavlenko A.V. Composite dental restorative and veneering materials in dentistry. Kniga plus. 2002; 224.

Korol M.D. Secondary deformities of dentitions. Poltava. 2003; 104.

Bida B.I. Principles of orthopaedic treatment of pathology in the dental system in case of reducing the height of the bite, its prognosis and prevention: thesis. Kyiv. 2003; 31.

Moldovanov A.G. Physiology and pathology of dental hard tissues abrasion. Tavrida. Simferopol. 1992; 186.

Nespryadko V.P. The organization of dental care for the Ukrainian population and ways of its reconstruction and improvement.Vestnik stomatoligiyi. 1997; 1: 16-19.

Hacker C. H., Wagner W.C., Razzoog M.E. An in vitro investigation of the wear of enamel on porcelain and gold in saliva. The Journal of prosthetic dentistry. 1996; 75(1): 14-17.

Koczorowski R., Wloch S. Evaluation of wear of selected prosthetic materials in contact with enamel and dentin. The Journal of prosthetic dentistry. 1999; 81(4): 453-459.

Engels J., Schubert O., Güth J.F. et al.Wear behavior of different double-crown systems. Clinical oral investigations. 2013; 17(2): 503-510.

Zhulev Ye.N. Porcelain-fused-to-metal dental prostheses: guideline. N.Novgorod. Izd-vo NGMA. 2005; 288.

Trezubov V.N., Shcherbakova A.S., Mishnev L.M. Propaedeutics of Prosthetic Dentistry. SPb. SpetsLit. 2004; 134.

Grishkina M.G., Ibragimov T.I., Kuropatova L.A. Modern methods of dental hard tissues preparation for all-ceramic dental prostheses. Sovremennaya ortopedicheskaya stomatologiya. 2004; 1: 84-85.

Remizov S.M. Determination of microhardness for the comparative evaluation of the dental tissues in healthy and affected teeth. Stomatologiya. 1965; 3: 33-37.

Morena R., Beaudreau G.M., Lockwood P.E. et al. Fatigue of dental ceramics in a simulated oral environment. Journal of dental research. 1986; 65(7): 993-997.

Wiley M.G. Effects of porcelain on occluding surfaces of restored teeth. The Journal of prosthetic dentistry. 1989; 61(2): 133-137.

Della Bona A., Kelly J. The clinical success of all-ceramic restorations. Journal of the American Dental Association. 2008; 139(4): 8-13.

Shirakura A., Lee H., Geminiani A. et al. The influence of veneering porcelain thickness of all-ceramic and metal ceramic crowns on failure resistance after cyclic loading. The Journal of Prosthetic Dentistry. 2009; 101(2): 119-127.

Esquivel-Upshaw J., Rose W., Oliveira E. et al. Randomized, Controlled Clinical Trial of Bilayer Ceramic and Metal‐Ceramic Crown Performance. Journal of Prosthodontics. 2013; 22(3): 166-173.

Suputtamongkol K., Anusavice K.J., Suchatlampong C. et al. Clinical performance and wear characteristics of veneered lithia-disilicate-based ceramic crowns. Dental Materials. 2008; 24(5): 667-673.

Ohlmann B., Trame J.P., Dreyhaupt J. et al. Wear of posterior metal‐free polymer crowns after 2 years. Journal of oral rehabilitation. 2008; 35(10): 782-788.

Etman M.K, Woolford M.J. Three-year clinical evaluation of two ceramic crown systems: a preliminary study. The Journal of prosthetic dentistry. 2010; 103(2): 80-90.

Mörmann W.H., Stawarczyk B., Ender A. et al. Wear characteristics of current aesthetic dental restorative CAD/CAM materials: two-body wear, gloss retention, roughness and Martens hardness. Journal of the mechanical behavior of biomedical materials. 2013; 20: 113-125.

Ma’an R., Rawa’a H. An evaluation of the effects of different polishing agents on the surface roughness of porcelain. Journal of Baghdad College of Dentistry. 2006; 18(2): 15-22.

Albashaireh Z.S., Ghazal M., Kern M. Two-body wear of different ceramic materials opposed to zirconia materials. The Journal of Prosthetic Dentistry. 2010; 104(2): 112-125.

Peregudov A.B. Diagnostisc of aesthetic violations and planning of complex rehabilitation in Clinic of Prosthetic Dentistry: thesis. M. 2006; 37.

De Aza A.H., Chevalier J., Fantozzi G. et al. Crack growth resistance of alumina, zirconia and zirconia toughened alumina ceramics for joint prostheses. Biomaterials. 2002; 23(3): 937-945.

Stober T., Geiger A., Rues S. et al. Factors affecting wear of composite resin denture teeth—24-month results from a clinical study. Clinical oral investigations. 2012; 16(2): 413-420.

Burgess J.O., Janyavula S., Lawson N.C. et al. Enamel wear opposing polished and aged zirconia. Operative dentistry. 2014; 39(2): 189-194.

Won-suck Oh, Ralph De Long, Kenneth J. Anusavice. Factors affecting enamel and ceramic wear: a literature review. Journal of prosthetic dentistry. 2002; 87(4): 451-459.

Park J.H., Park S., Lee K. et al. Antagonist wear of three CAD/CAM anatomic contour zirconia ceramics. The Journal of prosthetic dentistry. 2014; 111(1): 20-29.

Janyavula S., Lawson N., Cakir D. et al. The wear of polished and glazed zirconia against enamel. The Journal of prosthetic dentistry. 2013; 109(1): 22-29.

Mitov G., Heintze S.D., Walz S. et al. Wear behavior of dental Y-TZP ceramic against natural enamel after different finishing procedures. Dental Materials. 2012; 28(8): 909-918.

McLaren Edward A., Giordano II Russell A., Pober R. et al. Material testing and layering techniques of a new two phase all glass veneering porcelain for bonded porcelain and high alumina frameworks. Quintessence of Dental Technologies. 2003; 26: 69-81.

Metzler K.T., Woody R. D., Miller 3rd A.W. et al. In vitro investigation of the wear of human enamel by dental porcelain. The Journal of prosthetic dentistry. 1999; 81(3): 356-364.

Stober T., Bermejo J.L., Rammelsberg P. et al. Enamel wear caused by monolithic zirconia crowns after 6 months of clinical use. Journal of Oral Rehabilitation. 2014; 4: 314–322.




Copyright (c) 2017 Z. R. Ozhohan, A. V. Biben

Creative Commons License
This work is licensed under a Creative Commons Attribution-NonCommercial 4.0 International License.


IFNMU Logo

Free counters!